Resumo
Objectives: to evaluate the effect of sodium hypochlorite (NaOCl) treatment on dentin bonding by means of shear bond strength (SBS) measurements when using Prime&Bond NT (PB NT) adhesive. Ultrastructure of the interfaces was examined by scanning electron microscopy (SEM). Study design: Extracted human third molars were sectioned and ground to expose flat surfaces of superficial or deep dentin. Specimens were randomly assigned to two equal groups, and bonded as follows: (1) according to the manufacturers' directions, after 35% H3PO4 etching, (2) 5% NaOCl treated for 2 minutes, after 35% H3PO4 etching. Each sample was embedded in a Watanabe shear test assembly for a single plane lap shear. After PB NT bonding, specimens were stored in water for 24 h at 37°C and thermocycled (500x). Samples were tested in shear to failure using a universal testing machine at 0.75 mm/ min. Data were analyzed with ANOVA and Newman-Keuls multiple comparison test procedures. Two samples of each group were randomly selected to investigate the morphologic aspect of the resin/dentin interface with SEM. Results: After etching and after aqueous sodium hypochlorite (NaOClaq) application, SBS values were similar on superficial than deep dentin (p>0.05). SEM findings shows for H3PO4 etching conditioned samples a detectable hybrid layer and long resin tags; for NaOCl treated specimens, it may be observed a non apparent hybrid layer, and the adhesive contact directly with the neck of the cylindrical resin tags. Conclusions: The use of 5% NaOCl for 2 min after dentin demineralization when PB NT was employed did not improve the bond strength to dentin, probably due to nanofiller content and/or oxidative changes on collagen-depleted dentin.
Idioma original | ???core.languages.en_GB??? |
---|---|
Páginas (de-até) | 649-654 |
Número de páginas | 6 |
Revista | Medicina Oral, Patologia Oral y Cirugia Bucal |
Volume | 17 |
Número de emissão | 4 |
DOIs | |
Estado da publicação | ???researchoutput.status.published??? - jul. 2012 |